We believe this information is the best currently available on the subject. We offer it as a suggestion in any appropriate experimentation you may care to undertake. It is subject to revision as additional knowledge and experience are gained. We make no guarantee of results and assume no obligation or liability whatsoever in connection with this information. In case of conflict between standard and metric specifications, standard shall apply.
Download PDF| Property | Test Method | Standard | Metric |
| Base Fabric Type | ASTM D 751 | Polyester | Polyester |
| Base Fabric Weight | 6.5 oz/yd2 nominal | (220 g/m2 nominal) | |
| Thickness | ASTM D 751 | 30 mils min. | (0.76 mm min) |
| Weight | ASTM D 751 | 30.0 +- 2 oz./sq. yd. | (1017 +- 70 g/sq. m) |
| Tear Strength | ASTM D 751 Trap Tear |
40/55 lbs. min. | (175/245 N min.) |
| Braking Yield Strength | ASTM D 751 Grab Tensile |
550/550 lbs. min. | (2,447/2447 N min.) |
| Low Temperature Resistance | ASTM D 2136 4hrs-1/8" Mandrel |
Pass @ -30º F | (Pass @ -35º C) |
| Dimensional Stability | ASTM D 1204 100° C-1 hr |
0.5% max each direction |
|
| Hydrostatic Resistance | ASTM D 751 Method A |
800 psi min. | (5.51MPa min.) |
| Blocking Resistance | ASTM D 751 180° F |
#2 Rating max | #2 Rating max |
| Adhesion-Ply | ASTM D 413 Type A |
15 lbs./in. min. or film tearing bond |
(13 daN/5 cm min. or FTB) |
| Adhension-Heat Welded Seam | ASTM D 751 180° F |
40 lbs./2in. min. | (17.5 daN/5 cm min.) |
| Dead Load Seam Strength | ASTM D 751 4-Hour Test |
Pass 240 lbs/in. @ 70º F Pass 120 lbs/in. @ 160º F |
(Pass 980 N/2.54 cm @ 21º C) (Pass 534 N/2.54 cm @ 70º C) |
| Bonded Seam Strength | ASTM D 751 Procedure A, Grab Test Method |
550 lbs. min. | (2,450 N min.) |
| Abrasion Resistance | ASTM D 3389 H-18 Wheel 1kg Load |
2000 cycles min. before fabric exposure, 50 mg/100 cycles max. weight loss |
2000 cycles min. before fabric exposure, 50 mg/100 cycles max. weight loss |
| Weathering Resistance | ASTM G 153 | 8000 hours min. with no appreciable change or stiffening or cracking of coating |
8000 hours min. with no appreciable change or stiffening or cracking of coating |
| Water Absorption | ASTM D 471, Section 12 7 Days |
0.025 kg/m2 max. @ 70º F/21º C 0.14 kg/m2 max @ 212º F/100º C |
0.025 kg/m2 max. @ 70º F/21º C 0.14 kg/m2 max @ 212º F/100º C |
| Wicking | ASTM D 751 | 1/8" max. | (0.3 cm max.) |
| Bursting Strength | ASTM D 751 Ball Tip | 750 lbs. min. | (3330 N min.) |
| Puncture Resistance | ASTM D 4833 | 275 lbs. min. | 1200 N min. |
| Coefficient of Thermal Expansion / Contraction |
ASTM D 696 | 8 x 10- 6 in/in/º F max | (1.4 x 10- 5 cm/cm/º C max.) |
| Puncture Resistance | FTMS 101C Method 2031 | 350 lbs. (approx.) | 350 lbs. (approx.) |
Available Colors